How to Use a Pellet 3D Printer: PioCreat G5 Ultra, MS01 & G12 Guide

Article author: Eolas Prints
Article published at: Nov 26, 2026
Article tag: FGF Article tag: Guides Article tag: How-To Article tag: Pellet 3D Printers Article tag: Pellets Article tag: PioCreat Article tag: PioCreat G12 Article tag: PioCreat G5 Ultra Article tag: PioCreat MS01
PioCreat G5 Ultra pellet 3D printer with its pellet hopper, feed tube and screw extruder | Eolas Prints

A pellet 3D printer works like a filament printer with a different front end: plastic granules drop from a hopper into a heated screw, which melts them and pushes the melt through a large nozzle. To print well, you dry the pellets, preheat both heating zones of the screw, purge until the melt runs smoothly, and slice with thick layers, wide lines and little or no retraction. This guide takes you through each step on the three PioCreat machines we sell: the G5 Ultra, the MS01 and the G12.

Machine figures come from PioCreat's product pages and user manuals (G5 Ultra manual V2.2, G12 manual V6.2). Material figures come from our own pellet product pages. The settings tables are starting points to tune on your machine. If you are still choosing a printer, start with our pellet 3D printer buying guide.

In short

  • Feeding: all three machines take 2–5 mm pellets. The G5 Ultra has a 3 L hopper; the G12 has a 25 L hopper and a pneumatic conveyor that feeds the extruder, which needs compressed air above 0.6 MPa.
  • Two heating zones: the screw has an upper (feed) zone and a lower (melt) zone. Maximum nozzle temperatures are 420 °C on the G5 Ultra, 400 °C on the MS01 and 450 °C on the G12.
  • Dry first: dry PETG and rPET at 65–70 °C and TPU at 70–80 °C for 4–6 hours. Wet pellets cause bubbles, popping and stringing.
  • Slicer: PioCreat Slicer (Windows, free from PioCreat). PioCreat also lists Cura and Simplify3D for the G5 Ultra and G12.
  • Layers: 0.2–1.0 mm on the G5 Ultra, 0.5–1.5 mm on the MS01 and 0.6–2.0 mm on the G12. As a rule of thumb, start at about half the nozzle diameter.
  • Material changes: empty the barrel and purge until the new material runs clean, so plan your jobs in batches by material.

1. Pellet vs filament printing in 60 seconds

FGF (fused granular fabrication) is 3D printing straight from plastic pellets. A screw extruder is the rotating screw inside a heated barrel that conveys, melts and pressurises the pellets, doing the job of a filament printer's drive gears and hot end. Purging means pushing material through the screw until the melt coming out is clean, consistent and free of the previous material.

Filament printer Pellet (FGF) printer
Feedstock 1.75 or 2.85 mm filament on a spool 2–5 mm pellets poured into a hopper
Extrusion Gears push filament into a hot end A heated screw melts and pushes the pellets
Nozzles and layers Typically 0.4 mm nozzle, 0.1–0.3 mm layers 0.8–4.0 mm nozzles, 0.2–2.0 mm layers on these machines
Retraction Fast and precise Slow to respond; use little or none
Material change Unload one spool, load another Empty the hopper and barrel, then purge
Moisture Dry the spool when needed Dry the pellets before every job, at the rate the printer uses them

The pay-off is cheaper material and far higher output for large parts. For costs and payback, see the pellet 3D printer buying guide; for choosing a material, see our guide to 3D printing pellets.

2. Before you start: site, assembly and loading

Site and power

  • G5 Ultra: 765 × 890 × 1040 mm, 42 kg, 1450 W, AC 100–110 V or 220–240 V. It arrives as a base frame and a gantry frame that you assemble on site.
  • MS01: 870 × 1015 × 1995 mm, 274 kg, 4200 W, 100–120 V~ or 200–240 V~.
  • G12: 2135 × 1775 × 2305 mm, 750 kg, 7000 W on single-phase AC 220 V (an AC 110 V version exists for the US). The manual asks for a 3-core 4 mm² cable wired to the circuit breaker and compressed air above 0.6 MPa. Remove the four lifting rings after unpacking and before you power it on.

PioCreat's manuals ask for a well-ventilated, low-dust room away from heat sources, a stable floor without vibration and a grounded three-pin outlet. Never plug or unplug motor cables while the machine is on.

The three machines at a glance

G5 Ultra MS01 G12
Build volume 500 × 500 × 400 mm 500 × 500 × 650 mm 1200 × 1000 × 1000 mm
Nozzles supplied 0.8, 1.0 and 2.0 mm 1.0 mm (2.0, 3.0 and 4.0 mm optional) 1.2, 1.5, 2.0, 3.0 and 4.0 mm
Layer height 0.2–1.0 mm 0.5–1.5 mm 0.6–2.0 mm
Screw heating zones Upper up to 360 °C, lower up to 420 °C Dual-zone, up to 400 °C Upper up to 440 °C, lower up to 450 °C
Bed / chamber Up to 120 °C / open frame Up to 110 °C / enclosed, up to 100 °C Zoned, up to 130 °C / enclosed cabinet (no heated chamber specified)
Feeding 3 L hopper with sight window, feed tube to the screw, run-out detection Screw-fed hopper with run-out sensor 25 L transparent hopper, pneumatic conveyor, level sensors
Bed levelling 64-point laser See the supplied documentation 120-point laser
Slicer and files PioCreat Slicer, Cura, Simplify3D; USB drive, Wi-Fi PioCreat Slicer; USB drive PioCreat Slicer, Cura, Simplify3D; USB drive, Wi-Fi or wired network

Full specifications are on each product page. PioCreat has not published a public MS01 user manual, so follow the documentation that comes with the machine.

PioCreat G12 pellet 3D printer with its doors open, showing the 1200 x 1000 x 1000 mm build area
The G12 with its doors open: a 1200 × 1000 × 1000 mm build area inside an enclosed cabinet. Image: PioCreat.

Assemble and load the pellets

  • G5 Ultra: fit the display, the feed tube and feed port, the gantry, the pull rods and the Z-axis homing switch, then connect the cables as the manual shows. To load, check that the feed tube is connected, pour pellets into the hopper and close the lid. The sight window shows how much is left.
  • G12: check that the pneumatic conveyor at the bottom of the hopper funnel and the discharge pipe are connected, fill the storage hopper and close the lid. The Feeding button blows pellets into the barrel and switches off automatically after 15 seconds by default.
  • MS01: load the hopper as shown in the documentation supplied with the machine. The run-out sensor pauses the print when pellets run out and resumes once you refill.

3. Choose and dry your pellets

Start with PLA. It is the easiest material, and PioCreat's G12 manual asks you to use PLA pellets for the first test print. These are the figures from our pellet product pages:

Pellets Pellet size Nozzle Bed Drying
PLA 3.1–3.6 mm 190–220 °C 0–60 °C Less sensitive; if needed, dry at a low temperature (around 45–55 °C) so the pellets do not soften and stick
PETG 2–3.5 mm 230–250 °C 70–85 °C 65–70 °C for 4–6 h
TPU 93A 2.7–3.2 mm 220–240 °C 30–60 °C 70–80 °C for 4–6 h if exposed to humidity
ABS 2.8–3.2 mm 230–250 °C 90–110 °C Not stated on the product page; ask us before a long job
rPET (recycled) 2–3.5 mm 230–250 °C 70–85 °C 65–70 °C for 4–6 h

Each product page also links a technical datasheet with the resin's drying conditions for industrial desiccant dryers. PioCreat does not name PET for its printers, so treat rPET as a PETG-class material and run a test print first.

Why moisture matters more with pellets

PETG, rPET and TPU absorb water from the air. In the screw, that water turns to steam, so wet pellets print with bubbles, popping, stringing, rough surfaces and weak layers. A pellet printer also eats material fast: up to 0.8 kg an hour on the G5 Ultra and up to 3 kg an hour on the MS01 and G12. Your dryer has to deliver dry pellets at least that fast, or you will be printing wet material halfway through a long job.

  • Keep pellets in their sealed bag, with desiccant once opened, in a cool place below 50 °C.
  • Our practical advice: put only as much in the hopper as the printer will use in the next few hours, or feed it from a hopper dryer.
  • If a batch starts to pop or string partway through a job, dry it again before you change any slicer setting.
Trays of plastic pellets in white, black, green and red for pellet 3D printing
Plastic pellets in several colours. PioCreat's printers take 2–5 mm granules and can blend in colour masterbatch. Image: PioCreat.

4. Slicer setup

Install PioCreat Slicer and load the profile

  1. Download PioCreat Slicer from the Software Center on piocreat3d.com, or install it from the USB drive supplied with the printer. It runs on Windows.
  2. On first launch, the Configuration Wizard opens: choose your 3D printer, then your materials, then finish.
  3. Import the model (STL or OBJ; the G12 also takes 3MF), select the printer, the material and a configuration (a default one or your own), and slice. The G12 manual notes that slicing covers every model on the plate, so keep everything inside the build area.
  4. Check the G-code preview, save the file to the USB drive and print from the touchscreen, or send it over Wi-Fi.

PioCreat also lists Cura and Simplify3D for the G5 Ultra and G12. If you use one of them, copy the machine and material values from PioCreat Slicer's profile rather than starting from a filament printer profile.

Key settings

  • Nozzle, layer height and line width. A common rule of thumb is a layer height of about half the nozzle diameter, inside the machine's range, and a line width of 100–120% of the nozzle diameter.
  • Flow (extrusion multiplier). Screw output depends on the material, temperature and screw speed, so calibrate flow for each material and each new batch: print a single-wall test box, measure the wall with callipers and adjust flow until it matches the line width. During a print, the touchscreen lets you raise or lower flow, speed and Z-offset live.
  • Speed. Check volumetric flow, not just mm/s: speed × layer height × line width must stay below what the screw can melt. At its 0.8 kg/h rating, the G5 Ultra melts about 180 mm³ of PLA per second, which is about 80 mm/s with a 2.0 mm nozzle, 1.0 mm layers and 2.2 mm lines. The MS01 and G12 (3 kg/h) reach about 670 mm³/s, or about 76 mm/s with a 4.0 mm nozzle, 2.0 mm layers and 4.4 mm lines. These are maximum ratings, so start well below them. Print TPU at moderate speeds.
  • Retraction. A screw extruder reacts slowly to short reverse moves, and some pellet-extruder makers advise against retraction altogether. Start with the value in PioCreat's profile or with retraction off, cut down travel moves and use coasting or wipe if your slicer offers them. If the part still strings, dry the pellets and lower the temperature before adding retraction.
  • Temperatures. Set both zones. PioCreat's G12 manual says the lower zone is generally set about 10 °C hotter than the upper zone. A feed zone that runs too hot can soften pellets before they reach the melt zone.
  • Cooling. Thick beads hold a lot of heat. Use the part fan for PLA, keep it low for PETG, rPET and TPU, and off for ABS (our ABS datasheet gives 0%). On small or tall parts, set a minimum layer time so each layer can cool before the next.
  • First layer and brim. Print the first layer slowly, add a brim on large footprints and round off sharp corners.

Starting points: nozzle and layer height

Machine and nozzle Layer height Line width Use
G5 Ultra, 0.8 mm 0.4 mm 0.8–1.0 mm Finer detail
G5 Ultra, 1.0 mm 0.5 mm 1.0–1.2 mm First prints
G5 Ultra, 2.0 mm 1.0 mm 2.0–2.4 mm Fastest, largest parts
MS01, 1.0 mm 0.5 mm 1.0–1.2 mm Standard nozzle
G12, 1.2 mm 0.6 mm 1.2–1.4 mm Finer detail
G12, 2.0 mm 1.0 mm 2.0–2.4 mm General large parts
G12, 4.0 mm 2.0 mm 4.0–4.8 mm Maximum output

Starting points: material settings

Pellets Lower zone (nozzle) Bed Part fan Watch out for
PLA 190–220 °C 0–60 °C On Softens above about 55–60 °C in use
PETG 230–250 °C 70–85 °C Low Stringing when wet; bonds strongly to the bed
TPU 93A 220–240 °C 30–60 °C Low Uneven flow at high speed
ABS 230–250 °C 90–110 °C Off Warping; an enclosed, warm chamber is strongly recommended
rPET 230–250 °C 70–85 °C Low Test print first; slight colour variation between batches

Temperatures are from our pellet product pages; set the upper zone about 10 °C below the lower zone as a start. Tune everything on your own machine.

5. Your first print, step by step

  1. Prepare the bed. Clean the print surface with glass cleaner or isopropyl alcohol. On the G12, check that the fibreglass plate lies flat, lock it with the side screws and spread platform glue around the edge of the model's footprint (the centre does not need glue).
  2. Level and set the Z-offset. Run auto levelling from the touchscreen. On the G5 Ultra, if the readings differ by around 1 mm, turn the black knobs under the platform (clockwise for negative values, anticlockwise for positive), then level again. Set the Z-offset so the gap between nozzle and bed is about the thickness of a sheet of A4 paper (0.08–0.1 mm). Do not knock the feed tube or press on the platform while it levels.
  3. Load dry pellets. Fill the hopper with dried pellets and close the lid.
  4. Preheat. In the Preheat menu, set the upper and lower nozzle zones and the bed for your material. The G12 has PLA and ABS presets and custom values. The G5 Ultra bed reaches 60 °C in about 5 minutes and 90 °C in about 8.
  5. Purge until the flow is consistent. Choose an extrusion distance and speed and press Feed until the material comes out smoothly. Look for a steady, glossy strand with no bubbles and no traces of the previous material. Clear the purge with the supplied tools, never by hand.
  6. Start the print. Select the G-code file on the touchscreen and start.
  7. Watch the first layer. Adjust the Z-offset, flow and speed live from the print screen until the lines are flat, wide and touching.
  8. Monitor the hopper. Keep it topped up with dry pellets. The G5 Ultra and MS01 pause when pellets run out and resume after you refill; the G12's level sensors raise an alarm.
  9. Remove the part. Let it cool and wear gloves. Bend the flexible plate of the G5 Ultra to release the part. On the G12, use a scraper or undo the side thumb screws, slide the bed out, lift off the fibreglass plate and bend it; for large models, one person bends while another supports the part. The G12's front door stays locked while printing; unlock it from the home screen when the print is finished.
Laser levelling sensor on the PioCreat G5 Ultra measuring the distance from the print head to the bed
The G5 Ultra's non-contact laser sensor maps the bed at 64 points before you set the Z-offset. Image: PioCreat.
Removing a part from the PioCreat G12: loosen the screws, pull out the build plate and bend it to release the print
Releasing a part on the G12: loosen, pull out the plate, bend. Image: PioCreat.

6. Changing material and cleaning the screw

PioCreat's instruction is simple: before you print a different material, empty the residue in the barrel and extruder, then add the new material. The G5 Ultra has a quick-discharge system for this, and on the G12 the Eject command pulls material back into the barrel. A sequence that works:

  1. Let the hopper run nearly empty, then remove the pellets left in the hopper and feed tube.
  2. Keep both zones at the old material's temperature and extrude or discharge what is left in the barrel.
  3. Load the new material and purge until the strand is clean, the colour is uniform and there are no bubbles.
  4. Going from a hotter material to a cooler one (for example ABS or PETG to PLA): purge at the higher temperature first, then lower the zones step by step while purging. The old material will not melt properly at the new, lower temperature.
  5. Going from a cooler material to a hotter one: raise the temperature and purge straight away, so the cooler material does not sit and degrade in the hot barrel.

Purge with the incoming material, or with a natural or clear grade, which shows when the old colour has gone. Do not leave material sitting hot in a stopped screw: lower the temperatures during long pauses. Because every change costs material and time, plan jobs in batches by material and colour. PioCreat's G12 material-replacement video (below) shows the procedure.

PioCreat G12 screw extruder nozzle glowing hot during extrusion
The G12's segmented screw extruder heats up to 450 °C at the nozzle. Image: PioCreat.

7. Large parts: warping, cooling and orientation

  • Warping. Large flat parts shrink as they cool and lift at the corners. Use a brim, round off sharp corners, avoid solid infill on big flat bases and keep the printer away from doors and air-conditioning. On the G12, the bed heats the zones under the model automatically (up to 130 °C), and platform glue goes around the edge of the footprint.
  • Chamber. ABS and other warp-prone engineering materials need warmth around the part. The MS01's enclosed chamber holds up to 100 °C; the G5 Ultra is an open frame, so print ABS in a draught-free room and keep parts modest in size. Read more in open frame, enclosed or heated chamber.
  • Cooling and layer time. Wide, thick beads stay soft for longer. Tall, thin sections can sag when each layer is printed on top of a still-warm one, so set a minimum layer time or print two parts side by side.
  • Orientation. Put the largest flat face on the bed, keep overhangs moderate and avoid tall, slender features standing on their own.
  • One piece or split? The G12 prints up to 1200 × 1000 × 1000 mm in one piece. If a part is bigger than your machine, split it and join the sections with dovetails, dowel pins or bolted flanges, as covered in printing 1-metre parts in one piece.
PioCreat G12 zoned heated bed with heating zones up to 130 °C
The G12's zoned heated bed reaches up to 130 °C and heats only the zones under the model. Image: PioCreat.
PioCreat MS01 pellet 3D printer with its enclosed chamber heated to 100 °C
The MS01's fully enclosed chamber holds up to 100 °C to keep engineering materials from warping. Image: PioCreat.

8. Troubleshooting

Problem Likely causes What to do
Under-extrusion or uneven flow Wet pellets, empty or blocked hopper, upper zone too hot, lower zone too cold, speed above the screw's melt rate Dry the pellets, check the hopper and feed tube, keep the upper zone below the lower zone, raise the lower zone by 5–10 °C, slow down or raise flow
Bubbles, popping or hissing, rough surface Moisture in the pellets Dry at the temperatures in section 3 and keep the hopper covered
Stringing and oozing Wet material, temperature too high, long travel moves; the screw keeps pushing melt Dry first, lower the temperature by 5–10 °C, reduce travel and use coasting. See how to fix stringing and oozing
Warping or lifting Bed too cool, poor adhesion, draughts, sharp corners, ABS without an enclosure Brim, platform glue (G12), correct bed temperature, round corners, warm chamber for ABS. See first layer not sticking
Pellets bridging in the hopper or feed tube Damp pellets clumping, pellets outside 2–5 mm, heat creeping up into the feed zone, loose feed connections Check the pellet size, dry the pellets, lower the upper zone and check the feed tube; on the G12 check the conveyor and an air supply above 0.6 MPa
Nozzle clog Degraded material after a long time hot, contamination or dust in recycled material, changing to a cooler material without purging Purge hot, clean with the nozzle cleaner from the toolkit, replace the nozzle if needed
Weak layer bonding Temperature too low, too much cooling, long layer times on big parts, wet pellets Raise the lower zone, reduce the fan, print parts side by side, dry the pellets
File not found or not printing USB drive or slicing problem Wipe, format or replace the USB drive; move the model and slice again, or repair the model
Error message on the G12 Emergency stop, servo, temperature-loss or communication error Follow the on-screen tip: release the emergency stop and reboot, or check the heater, thermistor and board wiring, then restart

The G5 Ultra manual adds checks for axis motors, limit switches, levelling, the screen and the Z-axis coupler. If a fault remains after those checks, contact us.

9. Maintenance checklist

  • Before every print: clean the print surface with glass cleaner or isopropyl alcohol and check that the pellets are dry.
  • Regularly: with the power off, wipe dust and stray plastic off the frame, guide rails and wheels with a dry cloth. Clear debris from the hot end only with the supplied tools.
  • At every material change: empty the hopper and barrel and purge, as in section 6.
  • About every 3 months (G5 Ultra manual): grease the linear slide blocks through their grease nipples (PioCreat suggests oil of about 32–150 cSt) and grease the Z-axis lead screw with lithium soap grease with a dropping point of at least 258 °C.
  • Spares: nozzles and toolbox items are consumables and are not covered by the warranty, so keep spare nozzles in the sizes you use.

10. Official resources and videos

  • PioCreat's Software Center for PioCreat Slicer.
  • PioCreat product pages for the G5 Ultra, MS01 and G12.
  • The USB drive supplied with each printer holds the instructions, instruction videos and the slicer manual.

G5Ultra Pellet 3D Printer Operation Instruction (PioCreat): operating the G5 Ultra.

G12 Printing Material Replacement (PioCreat): changing material on the G12.

11. Frequently asked questions

How do you use a pellet 3D printer?

Dry the pellets, load them into the hopper, level the bed and set the Z-offset, preheat the upper and lower zones of the screw and the bed, then purge until the melt runs smoothly. Slice the model with thick layers and wide lines (for example 0.5 mm layers with a 1.0 mm nozzle), start the print and keep the hopper topped up with dry pellets.

Do pellets need to be dried before printing?

Yes for PETG, rPET and TPU: dry PETG and rPET at 65–70 °C and TPU at 70–80 °C for 4–6 hours. PLA is less sensitive; if needed, dry it at a low temperature of around 45–55 °C. The dryer must keep up with the printer: up to 0.8 kg/h on the G5 Ultra and up to 3 kg/h on the MS01 and G12.

Which slicer do PioCreat pellet printers use?

PioCreat Slicer, a free Windows program from PioCreat's Software Center that is also supplied on the printer's USB drive. Its Configuration Wizard sets up the printer and materials. PioCreat also lists Cura and Simplify3D for the G5 Ultra and G12.

What layer height should I use with a pellet 3D printer?

Start at about half the nozzle diameter and stay inside the machine's range: 0.5 mm with a 1.0 mm nozzle on the G5 Ultra (range 0.2–1.0 mm), 0.5 mm on the MS01 (0.5–1.5 mm) and 1.0 mm with a 2.0 mm nozzle on the G12 (0.6–2.0 mm).

Can you use retraction on a pellet 3D printer?

Only a little, if at all. A screw extruder reacts slowly to short reverse moves. Start with PioCreat's profile value or with retraction off, reduce travel moves and use coasting, and fix stringing by drying the pellets and lowering the temperature first.

How do I change material on a pellet 3D printer?

Empty the hopper and feed tube, extrude or discharge what is left in the barrel at the old material's temperature, then load the new material and purge until the strand is clean. When moving to a cooler material, purge hot first and lower the temperature step by step.

What size pellets do PioCreat printers take?

2–5 mm for the G5 Ultra, MS01 and G12. Eolas Prints pellets range from 2 mm to 3.6 mm: 3.1–3.6 mm for PLA, 2–3.5 mm for PETG and rPET, 2.7–3.2 mm for TPU and 2.8–3.2 mm for ABS.

Why is my pellet printer under-extruding?

The usual causes are wet pellets, an empty or bridged hopper, a feed zone that is too hot, a melt zone that is too cold, or printing faster than the screw can melt. Dry the pellets, check the feed, keep the upper zone below the lower zone and check the volumetric flow.

Buying a PioCreat printer or pellets from Eolas Prints

Eolas Prints, in Reocín, Cantabria (Spain), sells the PioCreat G5 Ultra, MS01 and G12 and the PLA, PETG, ABS, TPU and rPET pellets they run on, and makes its own filament from the same PLA, PETG, ABS and TPU pellets. We ship worldwide. Warranty is provided by the manufacturer, PioCreat, and processed through Eolas Prints.

See the G5 Ultra, MS01 and G12, all pellet 3D printers, and our PLA, PETG, TPU, ABS and rPET pellets. Read the pellet 3D printer buying guide, the guide to 3D printing pellets and the rPET pellets buyer's guide, or tell us what you want to print. We answer in English and Spanish.

Sources: PioCreat, G5 Ultra, MS01 and G12 product pages, Software Center, G5 Ultra user manual (V2.2) and G12 user manual (V6.2), and PioCreat's YouTube channel; Eolas Prints pellet product pages and technical datasheets; 3D Mag's pellet extruder guide for general FGF practice; checked 26 November 2026. Machine figures are PioCreat's and material figures are Eolas Prints'. Settings tables are starting points, not test results.

Share